Glass standard reference materials

 

Glass standard reference materials (SRM) are/were available at the National Institute of Standards and Technology (NIST) and the German Society of Glass Technology (DGG):

 

710A, Viscosity, Soda-lime-silica glass:

Page 1

Page 2

 

DGG I, Viscosity, Soda-lime-silica glass:

Composition and Viscosity Data (in German)

Measurement Details (in German)

Further Reference: G. Meerlender: "Viskositäts-Temperaturverhalten des Standardglases I der DGG"; Glastechn. Ber. (1974), vol. 47, no. 1, p 1-3 (in German)

 

711, Viscosity, Lead-silica glass:

Page 1

Page 2

 

712, 713, 714, Viscosity, various glasses:

Page 1

 

717A, Viscosity, Borosilicate glass:

Page 1

Page 2

Page 3

 

731, Thermal expansion, Borosilicate glass:

Page 1

Page 2

 

710, Viscosity, Soda-lime-silica glass

Reference: A. Napolitano, E. G. Hawkins: "Viscosity of a Standard Soda-Lime-Silica Glass"; J. of Research of the National Bureau of Standards - A. Physics and Chemistry (1964), vol. 68A, no. 5, p 439-448