Download Glass Property Calculation Software

Viscosity Calculator, 1.7 MB, after paper (3 MB) by Fluegel, 2007

Liquidus Temperature Calculator, 30 kB, after paper by Fluegel

Density at Room Temperature Calculator, 700 kB, after paper (137 kB) by Fluegel, 2007

Density and Thermal Expansion of Melts Calculator, 150 kB, after paper (230 kB) by Fluegel, 2005

Thermal Expansion below Tg Calculator, 250 kB, after paper (360 kB) by Fluegel, 2006

Hydrolytic Class Calculator, 200 kB

Shear Modulus Calculator, 200 kB

Electrical Conductivity of Melts Calculator, 400 kB, after paper (340 kB) by Fluegel et al., 2005

Water Solubility in Melts Calculator, 100 kB, after paper by Fluegel et al., 2005

Thermal (Phonon) Conductivity Calculater, 26 kB, after paper by Choudhary et al., 2005

Surface Tension Calculater, 26 kB, after paper by Kucuk et al., 1999



Optimization of Several Glass Properties

Optimization Demo, 200 kB



Glass batching

Batch Calculator Demo, 160 kB

Conversion from wt% to mol% and vice versa, 30 kB